The general use environment of nickel-based alloy is mainly acid (such as sulfuric acid, hydrochloric acid, hydrofluoric acid, phosphoric acid, nitric acid, organic acid), alkali, salt, atmosphere, water, halogen or halide (such as fluorine and hydrogen fluoride, chlorine and hydrogen chloride).The corrosion of different nickel-based alloys in each environment is different, and the actual application is often a variety of environments coexist, so the reasons for corrosion are also diverse.
Nickel-based alloy is prone to a variety of corrosion in the process of use, the main performance of the following:
Uniform corrosion, local corrosion (such as pitting corrosion, gap corrosion, bacterial corrosion), environmentally sensitive cracking (such as corrosion fatigue, stress corrosion cracking, liquid metal cracking, hydrogen embrittlement), intercrystalline corrosion, erosion corrosion, electrochemical corrosion, dealloy corrosion, etc.
Uniform corrosion - uniform corrosion is a balanced corrosion, is the most common type of corrosion.Characterized by consistent chemical and electrochemical reactions across the exposed surface of the workpiece, the metal becomes thinner and thinner, eventually leading to failure.
Local corrosion - corrosion that occurs in a specific local area or under specific conditions, especially in a local area.Pitting, interstitial corrosion and bacterial corrosion are all manifestations of local corrosion.
Pitting - pitting is a concentrated corrosion of a metal that leads to the appearance of pits.Although these pits are very small in their early stages, if not taken seriously, they can spread very quickly, causing metal penetration in the short term and eventually failure.
Gap corrosion - gap corrosion usually occurs in two surfaces (such as gaskets and fasteners) between the very small gap.Compared with pitting, the microscopic environment inside the void is completely different from the surrounding environment.The concentration difference cell will cause the gap corrosion to proceed very quickly.
Bacterial corrosion - bacterial corrosion is a recently recognized type of localized corrosion.Some bacteria form dome-shaped colonies that cling to metal surfaces.The structure of the flora is completely isolated and sealed from the outside.The life cycle of these bacteria creates a corrosive environment within the flora that corrodes the metal.Bacterial corrosion usually occurs in parts that come into contact with natural water (not fresh or salt water) and can also occur in industrial systems where water is used for production purposes.
Environmentally sensitive cracking - some corrosion is due to the chemical state of the environment and the mechanical state of the metal itself.These two states must be present at the same time, in order to form environmentally sensitive cracking.Corrosion fatigue, stress corrosion cracking, liquid metal cracking and hydrogen embrittlement are the specific types of environmentally sensitive cracking.
Corrosion fatigue - corrosion fatigue failure is due to the corrosion of the medium leading to the metal fatigue resistance.In general, it does not show significant metal degradation, but premature failure of components under cyclic conditions.The stress at which the element fails is not sufficient to invalidate the metal.
Stress corrosion cracking - mainly refers to cracking caused by the presence of both tensile stress and corrosive medium.In such cracking, tiny cracks spread outward through the corrosion point, while most of the surface of the metal is not actually corroded.Chloride stress cracking of stainless steel and ammonia stress cracking of nickel-copper alloy are examples of stress corrosion cracking.
Liquid metal cracking - liquid metal cracking is a special type of stress corrosion.Sensitive metals (usually due to residual tensile stress during manufacturing) are corroded (cracked) by liquid metals with low melting points.For example, cracking of aged ni-cr-fe alloys is caused by silver - based brazing.
Hydrogen embrittlement - hydrogen embrittlement is mainly caused by the infiltration of hydrogen elements.Hydrogen embrittlement may result from the formation of hydrides or from the dissolution of hydrogen atoms.Whatever its mechanism, hydrogen embrittlement leads to the formation and diffusion of tiny cracks and holes in the metal structure.
Intercrystalline corrosion - intercrystalline corrosion, as the name implies, is a selective corrosion of metal compounds in the grain boundary by a corrosive medium.Several conditions can lead to intercrystalline corrosion of metal materials.In some environments, the grain boundaries of metals are relatively active because metal compounds tend to precipitate and move to the grain boundaries during thermal machining.If these compounds are more active than metal substrates, they will be selectively corroded.The metal reaction will cause the depletion of some elements in the adjacent area of grain boundary, thus making this area less resistant to corrosion.An example of intergranular corrosion is often encountered because of the formation of chromium carbide precipitation, resulting in the depletion of chromium, which leads to the corrosion of unstable austenitic stainless steel.
Scour corrosion - scour corrosion refers to the relative movement of the corrosive medium and the metal surface, which causes the metal to corrode faster.Usually, this movement is rapid and involves mechanical wear or abrasion.Metal on the surface is dissolved and carried away in the form of ions or corrosion products on the metal surface are washed away.
Electrochemical corrosion - electrochemical corrosion results from the electrical coupling between two different types of metals in the corrosion medium, resulting in corrosion of non-corrosion resistant metals.The difference in metal may be due to the difference in structure and structure, with the active metal becoming the anode and the inert metal becoming the cathode.The anode metal actually protects the cathode by sacrificing itself.The further apart the two materials are in the electrochemical sequence, the greater the possibility that the active metal will be corroded.